Ceramics-Silikáty 40, (4) 131 - 136 (1996)


EFFECT OF GRINDING OF Y₂O₃, BaCO₃ AND CuO ON SYNTHESIS OF YBa₂Cu₃O₇
 
Plešingerová Beatrice 1, Buchal Antonín 2, Šepelák Vladimír 3, Tkáčová Klára 3
 
1 Department of Chemistry, Faculty of Metallurgy, Technical University Košice, Letná 9, 042 00 Košice, Slovak Republic
2 Institute of Material Engineering F. Píška, Technical University, Faculty of Mechanical Engineering, Technická 2, 616 60 Brno
3 Institute of Geotechnics, Slovak Academy of Sciences, Watsonova 45, 043 53 Košice, Slovak Renublic

The very fine and surface reactive powder mixture was prepared by highly intensive short time mill grinding of the components Y₂O₃, BaCO₃ and CuO. Pure YBa₂Cu₃O₇ created by reaction of the components of grinding mixture at temperature 900 - 950°C. The temperature of the synthesis of YBa₂Cu₃O₇ decreased owing to the grinding about 50 to 100°C. Lower temperature of the synthesis had a positive effect on the purity of the final product.