Ceramics-Silikáty 57, (4) 290 - 296 (2013) |
|
STRUCTURAL AND DIELECTRIC STUDIES ON Sr0.5-3y/2LayBa0.5Nb2O6 CERAMIC SYSTEMS WITH VARIED SINTERING TIME AND La CONCENTRATION |
Zahariman S. R., Velayutham T. S., Abd Majid W. H.,
Said Mardhian,
Gan W. C. |
Low Dimensional Materials Research Centre, Physics Department,
University of Malaya, 50603 Kuala Lumpur, Malaysia
|
Keywords: Dielectric properties, Curie temperature, Microstructure, Density |
Sr0.5Ba0.5Nb2O6 (SBN50) ceramic doped with different concentration of Lanthanum, La according to stoichiometric formulation
of Sr0.5-3y/2LayBa0.5Nb2O6 (LSBN) with y = 0.01, 0.03, 0.05 and 0.07 prepared using traditional ceramic method
at the calcination temperature of 1200oC and sintered at 1300oC at varied sintering time. The effects of the sintering time
and La3+ substitution on the morphological, compositional, structural and electrical properties of the LSBN is presented
using scanning electronic microscopy (SEM), energy dispersive spectroscopy (EDS), X-ray diffraction (XRD) and dielectric
analysis. The XRD spectra confirm the presence of TTB structure in the ceramics. The Curie temperature (Tc) of the ceramic
identified from the dielectric studies performed in the temperature range of 28oC to 300oC. The temperature dependent
dielectric exhibits broad peaks indicating a diffuse phase transition and relaxor behavior of the ceramic. The measured
density of the samples is proportional to the sintering time and inversely proportional to the amount of the La3+ substitution.
The solubility limit of La3+ ions in the SBN solid solution is at y ~ 0.05. This observation is also supported by the dielectric
results where the dielectric properties of the ceramic deteriorate for y > 0.05 La substitution. |
PDF (1.7 MB) |
|